Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.27 J/cm | 4.25 ft-lb/in | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Izod Impact, Notched | 2.27 J/cm | 4.25 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH7010HF PPE+PS Noryl* NH7010HF resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight par.. |
|||
Izod Impact, Notched | 2.27 J/cm | 4.25 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2644 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled for auto application |