Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 13.3 J/cm | 24.9 ft-lb/in | ASTM D256 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Izod Impact, Notched | 13.3 J/cm | 25.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 13.3 J/cm | 25.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Izod Impact, Notched | 13.3 J/cm | 25.0 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 13.3 J/cm @Thickness 3.17 mm |
25.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2502 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 13.3 J/cm @Thickness 3.17 mm |
25.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2506 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 13.3 J/cm | 25.0 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P-10TC-1777 10% Talc Filled, UV Stabilized Polypropylene Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 13.3 J/cm @Thickness 3.17 mm |
25.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2503 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |