Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.86 - 6.94 J/cm @Temperature -40.0 - -20.0 °C |
3.48 - 13.0 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 3.51 J/cm Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature -40.0 °C |
3.48 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature -30.0 °C |
3.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Izod Impact, Notched | 1.86 J/cm | 3.49 ft-lb/in | |
Shinil Chemical SHINCON ABS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0300 ABS, Unreinforced FR Flame-retardant non-halogen ABS with superior heat resistance that can be used in the interior/exterior material of CD/DVD-Combo and DVD-RecordersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0926 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 6.35 mm |
3.49 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0300 ABS, Unreinforced FR Flame-retardant non-halogen ABS with superior heat resistance that can be used in the interior/exterior material of CD/DVD-Combo and DVD-RecordersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0926 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 6.35 mm |
3.49 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature 23.0 °C |
3.48 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX917 PPE+PS+PA This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature -40.0 °C |
3.48 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1543 PPE+PS |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature -40.0 °C |
3.48 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1543 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 1.86 J/cm @Thickness 3.17 mm |
3.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
Izod Impact, Notched | 1.86 J/cm | 3.49 ft-lb/in | ASTM D256 |
Cheng Yu Plastic E500G20 PC/PET, 20% Glass Fiber |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature 23.0 °C |
3.48 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Izod Impact, Notched | 1.86 J/cm @Temperature -30.0 °C |
3.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East) Blow moldable, impact modifed XENOY |
|||
Izod Impact, Notched | 1.86 J/cm | 3.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |