Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® BC 82 High Density Polyethylene - Blow Molding Eraclene BC 82 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC B5429/B5429A High Density Polyethylene for Blow Molding Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC M40060 Series High Density Polyethylene for Injection Molding Product Description: M40060 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
Izod Impact, Notched | >= 1.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 3.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Styrolution Polystyrol 495 F GR 2 PS Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180 |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180 |
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Toyobo T-772 Nylon, Plating Grade Key Feature: Plating grade; Glass fiber and mineral reinforced grades; thermal and impact resistantInformation provided by Toyobo Co., Ltd |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM 45% Glass Fiber Reinforced, High Strength.Information provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |