Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.57 J/cm | 2.94 ft-lb/in | ASTM D256 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Izod Impact, Notched | 1.57 J/cm | 2.94 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HM2604AW PA6+GF60% Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
2.94 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D256 |
Global HI-830 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Izod Impact, Notched | 1.57 J/cm | 2.94 ft-lb/in | ASTM D256 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm | 2.94 ft-lb/in | |
Zylog Hipolyene® 6251 Y M2 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.57 J/cm @Temperature 23.0 °C |
2.94 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Denka MALECCA K-510 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Izod Impact, Notched | 1.57 J/cm | 2.94 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250G60 60% Glass Fiber Reinforced, High Modulus PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUXY KS G55 Amorphous PA6 Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical |