Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.56 J/cm | 2.92 ft-lb/in | ISO METHOD 180 |
NYCOA 567 PA 6 plasticized general purpose molding and extrusion grade used in shoe heels and mono.Information provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 1.56 J/cm @Temperature -30.0 °C |
2.92 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EX1332T PC Lexan* EX1332T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and is UV stabilized. It is availab.. |
|||
Izod Impact, Notched | 1.56 J/cm @Temperature 23.0 °C |
2.92 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 1.56 J/cm | 2.92 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific) PPE+PS, 115 oC HDT |