Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.46 J/cm | 2.74 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.46 J/cm | 2.74 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12 LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 1.46 J/cm @Temperature 23.0 °C |
2.74 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Denka MALECCA K-600 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |