Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Multibase Nylex™ 2185 HF Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Reliance Industries Reclair R35042 Polyethylene Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Flint Hills P6G4Z-097 Impact Copolymer Polypropylene Features: Good impact/stiffness balance. Product does not contain animal derived components.Applications: Injection Molding - appliance components, consumer durables, caps and closures.Informatio.. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® ABS 8005 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 LNP* THERMOCOMP* RF009H is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | SOP-MEC-002.01 |
Ex-Tech Plastics PerformaTech™ PVC XAS-11 Low Charging PVC Engineered for packaging applications that contain non-ESD sensitive items to be transported within ESD controlled environments, PerformTech XAS-11 is a low charging (formerly known as anti-static) .. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | SOP-MEC-002.01 |
Ex-Tech Plastics PerformaTech™ PVC XSD-28 Static Dissipative PVC Manufactured in thickness from 10 to 60 mils, PerformTech XSD-28 is available in rigid vinyl or PET. XSD-28 is a static dissipative sheet engineered specifically for ESD sensitive packaging for use .. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
ExxonMobil PP7035E5 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polycarbonate POL051G20L Glass Reinforced |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature 23.0 °C |
2.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp PF007 PA 6 (Asia Pacific) LNP* Thermocomp* PF007 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 (Asia Pacific) LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature 23.0 °C |
2.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |