Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 600 A 44 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-220 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 4950 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | BS 2782.306A |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Loxim 330 01HSL Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific) LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | |
Sanyo PELESTAT® NC6321 ABS (12wt%) PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a va.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA303G43 Nylon 6.6, 43% Glass Fiber 43% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB300G7 Nylon 6, 35% Glass Fiber 35% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |