Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
NYCOA 27/300SR Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PC-30GF/000 BLACK Polycarbonate (PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -30.0 °C |
2.44 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -30.0 °C |
2.44 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -29.0 °C |
2.44 ft-lb/in @Temperature -20.2 °F |
|
Spartech Spectrum® S370 TPO Polyolefin Sheet
(discontinued **) Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -30.0 °C |
2.44 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -30.0 °C |
2.44 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.17 mm |
2.44 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | 23° C; ASTM D256 |
Flint Hills AP6120-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature 23.0 °C |
2.44 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 1.30 - 1.50 J/cm | 2.44 - 2.81 ft-lb/in | ASTM D256 |
Loxim 130 01V0 Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Izod Impact, Notched | 1.30 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.44 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm Notch Depth; ASTM D256 |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature -30.0 °C |
2.44 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt.. |
|||
Izod Impact, Notched | 1.30 J/cm @Temperature 23.0 °C |
2.44 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamLloy PA917G6 PP/NYLON 66 alloy, 30% Glass Fiber 30% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-B30 PTFE Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 4233 B ABS Utility GradeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proces.. |
|||
Izod Impact, Notched | 1.30 J/cm | 2.44 ft-lb/in | ASTM D256 |
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.30 - 1.30 J/cm @Temperature -40.0 - -40.0 °C |
2.44 - 2.44 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.30 J/cm Grade Count:2 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |