Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256-56 |
Rotuba 860H Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 23.0 °C |
2.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coeffi.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 6.35 mm |
2.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Kostat ICP-STAT ICS-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Heat Stabilized, Good UV.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PC GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | 1/4 in. at 73°F; ASTM D256 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |