Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.90 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Izod Impact, Notched | 1.01 - 1.07 J/cm @Temperature -20.0 - -20.0 °C |
1.89 - 2.00 ft-lb/in @Temperature -4.00 - -4.00 °F |
Average value: 0.864 J/cm Grade Count:2 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.18 mm |
1.89 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® EFL-4544 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched | 1.01 - 6.51 J/cm | 1.90 - 12.2 ft-lb/in | Average value: 1.97 J/cm Grade Count:57 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific) LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66 LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® EG106 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Total PSI 740 Polystyrene Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding. It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, suc.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature -40.0 °C |
1.89 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | 1/4 in. at 73°F; ASTM D256 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA T-115 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
E-Polymers Tekaster® F615G30 , 30% Glass Fiber Reinforced PET 30% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | compression molded; ASTM D256 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |