Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.990 J/cm @Temperature 23.0 °C |
1.85 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su.. |
|||
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant. |
|||
Izod Impact, Notched | 0.990 J/cm @Temperature 23.0 °C |
1.85 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.990 J/cm @Temperature -30.0 °C |
1.85 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PVX516 PPE PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT |
|||
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6 LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P1503 Polycarbonate A rigid flame retardant polycarbonate, UV stabilized for applications requiring superior dimensional stability and overall toughness. Also available as 1500 without UV stabilizer.Data provided by t.. |
|||
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1503WO BK Polycarbonate A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.990 J/cm | 1.85 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2935 PPE+PS (Asia Pacific) PPE/PS, GF20%, non-FR |