Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-2001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 808 C8 WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 23.0 °C |
1.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers 30GF 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.20 mm, Temperature 22.8 °C |
1.80 ft-lb/in @Thickness 0.126 in, Temperature 73.0 °F |
injection molded ASTM Type 1 specimen; ASTM D256 |
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NL-20GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.961 - 2.14 J/cm | 1.80 - 4.00 ft-lb/in | Average value: 1.40 J/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
I. Stern BLK100 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetProfilesAgency Rating.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-240 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® NY-7/EC NAT PA6 |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® HIPS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256A |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NPP 808 C8 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFPC 5040 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |