Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | 0.125 in.; ASTM D256 |
Resirene Resirene® 4220 High Impact Polystyrene Features:High FlowEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityExternal LubricatedApplications:InjectionTV CabinetsTyping Machine CasesPrintersToysInformation provided by US distributor Cals.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1204 33 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ineos ABS Centrex® 401 AES Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -50.0 °C |
1.70 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Dow Retain® 8209 ABS + Polycarbonate Data provided by Dow Chemical. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 109 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 425 Polyester - PBT, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 124 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.910 J/cm | 1.70 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® L935 Nylon 11 An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.910 - 1.17 J/cm @Thickness 6.35 mm |
1.70 - 2.19 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 0.910 - 0.910 J/cm @Temperature -40.0 - -40.0 °C |
1.70 - 1.70 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.910 J/cm Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |