Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP521-187 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9779 Medium Grey Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF15 IM1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® PC FR BK Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PET GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 22.8 °C |
1.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene GPP1640 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 40% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRF 2704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance; Good Processability Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Te.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene Medium Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 2550A is a medium impact, high flow, controlled rheology copolymer of polypropylene designed for such .. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P-25FG-3809 25% Glass Fiber Reinforced Information provided by Asahi Thermofil |