Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL16E PC LNP* Lubricomp* DFL16E is a compound based on Polycarbonate resin containing 30% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Notched | 0.900 - 1.00 J/cm | 1.69 - 1.87 ft-lb/in | ASTM D256 |
Loxim 330 01V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA 6/10 LNP LUBRICOMP* QFP36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wesr Resistant. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2200R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC (Asia Pacific) LNP* STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® HR426 PBT AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm |
1.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6425 9885 Abrasion Resistant Polystyrene Characteristics Low friction, impact polystyrene to provide wear resistance and static charge dissipation Excellent gloss & molded appearance and weld line miscibility Easy flowing grade with good.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced with molybdenum disulfide polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV300G4 ABS, 20% Glass Fiber 20% glass fiber reinforced, heat resistant and minimal mold shrinkage ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB847I4 Nylon 6, 20% Glass Fiber and Mineral 20% glass fiber and mineral reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.17 mm |
1.69 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP30-2400 GF20 20% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® T80G20 , 20% Glass Fiber Reinforced PBT/ABS Alloy 20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.900 J/cm @Diameter 3.17 mm |
1.69 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |