Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | Notched/Unnotched not specified; ASTM D256A |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Izod Impact, Notched | 0.883 - 1.12 J/cm | 1.65 - 2.10 ft-lb/in | Average value: 0.970 J/cm Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID SG2600B PA6+GF60%, General purpose, Good Surface Feature: Injection Molding, PA6+GF60%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
Izod Impact, Notched | 0.883 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 6.35 mm |
>= 1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | |
Shinil Chemical SHINSTRA PC/ABS SCV2030 Structural Polymer Housing SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HT-8200G MPPE/PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-1150G PC/ABS, 15% Glass Filled FR 15% GF reinforcement; can be used in mold frames for LCD BLU.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210G25 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G25 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5400G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NG1300S Nylon 66, 30% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256 |
Cheng Yu Plastic IPS610BK Electric Conducting HIPS, Extrusion |
|||
Izod Impact, Notched | 0.883 - 1.87 J/cm | 1.65 - 3.50 ft-lb/in | Average value: 1.38 J/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256A |
Total Lacqrene® 814(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformati.. |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 6.35 mm |
>= 1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 6.35 mm |
>= 1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print.. |
|||
Izod Impact, Notched | >= 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |