Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256A |
DSM Somos® 8110 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
Kolon KOCETAL® EL302 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
Kolon KOCETAL® K100 Standard Grade Acetal Resin Suitable for extrusion and injection molding of thick products. Applications: Extruded use such as rod, pipe, tube, and sheetInformation provided by API Kolon. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256A |
LyondellBasell Adsylâ„¢ 5C30F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256A |
LyondellBasell Adsylâ„¢ 5C37F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON 9X08403C Liquid Crystal Polymer (LCP) LNP* STAT-KON* 9X08403C is a compound based on Liquid Crystal Polymer (LCP) resin containing Carbon Fiber. Added features of this material are: Clean Compounding System, High Temperature, Flame Re.. |
|||
Izod Impact, Notched | 0.870 J/cm | 1.63 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific) PPE+PS GF20% High Heat FR V-0 |