Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.801 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 is a 45% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: .. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 2003 TI Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PK-20CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5430 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF20 L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP 0159 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, .. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® B5536 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437T40L Talc Reinforced |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-20FG-0600 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.801 J/cm @Temperature 22.8 °C |
1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA111G30IF Nylon 66, 30% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA4/6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant and Heat StabilizedTPCI# 8277150Information provided by TP Composites, Inc. |