Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax SV954 Polypropylene Impact Copolymer Key Features: nucleation shortens cycles for higher productivity, resists dirt and dust pick-up, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling an.. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature 23.0 °C |
1.37 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE003M PC LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -20.0 °C |
1.37 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM-D256 |
Braskem IA59 HDPE Injection Molding Polyethylene Homopolymer IA59 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high processability and low warpage and contai.. |
|||
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.730 J/cm @Temperature -30.0 °C |
1.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent, OQ Quality |