Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.670 J/cm @Temperature 23.0 °C |
>= 1.26 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
Ineos T60-500 HDPE T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog.. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Izod Impact, Notched | 0.670 J/cm @Temperature -30.0 °C |
1.26 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched | 0.670 J/cm @Temperature -30.0 °C |
1.26 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX04522C PC (Asia Pacific) LNP Stat-Kon DX04522C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: High Modulus, Electrically Conductive, Clean Compound System. Also .. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66 LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66 LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66 LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66 LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66 LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Izod Impact, Notched | 0.670 J/cm @Temperature -30.0 °C |
1.26 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.670 J/cm | 1.26 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |