Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Multibase Nylex™ 2185 FR V0 Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Ovation Polymers RIGITRON 10020 GF Polycarbonate, 20% Glass Reinforced PC - Glass reinforced (20 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor.. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Ovation Polymers RIGITRON 20433 GF PBT, 33% Glass Reinforced PBT - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Izod Impact, Notched | 0.667 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.25 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Izod Impact, Notched | >= 0.667 J/cm | >= 1.25 ft-lb/in | Method A; ASTM D 256 |
Karina E 854-35/9-A-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform.. |
|||
Izod Impact, Notched | 0.667 - 1.07 J/cm | 1.25 - 2.00 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Izod Impact, Notched | >= 0.667 J/cm | >= 1.25 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Izod Impact, Notched | 0.667 J/cm | 1.25 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® TFIPP 2020 High Impact Talc Filled Polypropylene AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |