Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Izod Impact, Notched | 0.650 - 0.800 J/cm | 1.22 - 1.50 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MQ 70 U High Density Polyethylene - Injection Molding Eraclene MQ 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a mediu.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM Data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GE 4960 BR HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.650 - 0.750 J/cm | 1.22 - 1.41 ft-lb/in | ASTM D256 |
Loxim 230 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.22 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.22 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.20 mm |
1.22 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -30.0 °C |
1.22 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm @Thickness 3.17 mm |
1.22 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PW300G7 SAN, 35% Glass Fiber 35% glass fiber reinforced SAN for very high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature 23.0 °C |
1.22 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1109 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.650 J/cm @Temperature -20.0 °C |
1.22 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4624WZ Polypropylene, Impact Copolymer ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce.. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 J/cm | 1.22 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 6630 Nylon 6.6 Polypropylene Alloy DescriptionPolyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.650 - 2.94 J/cm | 1.22 - 5.50 ft-lb/in | Average value: 1.21 J/cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |