Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.641 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® DB-5/SS/10 Polycarbonate, 10% Stainless Steel Fiber (dry blend) |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF15 HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformat.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFPPCC-10 10% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled |