Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
NYCOA 2025 Nylon 6 extrusion and molding grade with mold release and quicker cycle times for sports cleatsInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ NT-818.G002-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 A HS Natural A Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PI-30GF/000R BLACK Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba M Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba MH Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 6.35 mm |
1.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp ZFL34XXC PPE+PS LNP LUBRICOMP* ZFL34XXC is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC (Asia Pacific) LNP* Thermocomp* DX06411 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-1201 TF10 10% Talc Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature -40.0 °C |
1.20 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Conditioned) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials.Data provided by the manufacturer, .. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 461 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R190B Acetal General purpose reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. Black. Available in UV stabilized grades: R190-B2 (good weatherability); R190-H2B (maximum weatherab.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R528LW Nylon 66 General purpose injection molding grade Nylon 66, lubricated and FDA approved.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® RH190H2-B Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized with carbon black for outstanding weatherability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.640 J/cm @Diameter 3.17 mm |
1.20 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 4501 Medium Impact Polystyrene