Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol R110MK Polypropylene REPOL Polypropylene R110MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ISO 179 |
Gharda Chemicals GATONE™ 5600 PEEK, Low Viscosity Grade
(discontinued **) Low viscosity. grade for injection molding of thin sections & complex partsCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellen.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 - 3.20 mm |
1.12 - 1.50 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.600 - 1.12 J/cm @Temperature -30.0 - -30.0 °C |
1.12 - 2.10 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.864 J/cm Grade Count:9 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Izod Impact, Notched | 0.600 - 0.650 J/cm | 1.12 - 1.22 ft-lb/in | ASTM D256 |
Loxim 235 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene Characteristic: 30%wt of Sulfate Barium filled, high gloss, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SPS Guang Zhou POBUXâ„¢ 3001EPG15 Non-halogen flame retardance/GF15%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm |
1.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6411 1924 Light Stabilized Polystyrene Characteristics Prevents dust patterns due to static charges High gloss Good flow Improved light fastness Processing Injection molding Extrusion Applications A/C and cooler grill Material Status.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM-D256 |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16769N Internally Lubricated, Glass Fiber Reinforced PPS Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Temperature 0.000 - 0.000 °C |
1.12 - 1.50 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.468 J/cm Grade Count:4 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1013 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |