Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 6.35 mm |
1.10 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.10 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.10 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® AS-20GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe.. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256-A |
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA) Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr.. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ISO 180 |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ CN30XT Nylon 610 Isocorâ„¢ CN30XT is a low viscosity PA-610 based copolymer. This transparent nylon resin is specifically suited for applications requiring increased solvent resistance and UV stability. Isocor.. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF14 L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 NAT Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 1026102Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF/M30 HS BK 10/20% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 22.8 °C |
1.10 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS HI 0230 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 HS L Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PBT GF15 WT 096 LE 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: WhiteTPCI# 6862111Information provided by TP Composit.. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® 930L Nylon 6 (DAM) Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli.. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® SKG20 20% GF ABS Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast.. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256A |
Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin Clarity. TOTAL Polypropylene M3382MZ produces thermoformed parts with superior clarity, gloss and excellent side wall stiffness.Recommended Applications. TOTAL Polypropylene M3382MZ is ideal for d.. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 22.8 °C |
1.10 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant ABS4500G10BK ABS, 10% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336G25M5CL Glass/Mineral Reinforced Coupled |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-35FM-1309 35% Glass and Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFN 6013 Glass Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6 PA6 GR15 WF25 Glass/Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |