Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Plenco 50240 PET, Pellet, Injection Molded, Blue
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Ineos T50-800 HDPE T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use .. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256A |
LyondellBasell Astryn NXO-21001 Polypropylene Copolymer Key Features: high melt flow, medium modulus polypropylene copolymer, high flow, excellent processability, excellent colorabilityApplications: wire harnesses, housings, thin walled partsDescription:.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific) LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing Bearing Grade. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC (Asia Pacific) LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Asia Pacific) LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP XFL21R PA LNP* LUBRICOMP* XFL21R is a compound based on Amorphous Nylon resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Mold Release. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML3260 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL APS440 PPE+PPS (Asia Pacific) |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific) LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |