Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 A Zip 23 Natural 1 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.530 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® NI-10GF/000 Polyamide 610 (Nylon 610) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 75F4-2 Polypropylene Copolymer, 20% Talc Key Features: conventional melt flow, medium high modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aestheticsApplications: small appli.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256A |
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small.. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFL32L Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL32L is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.This data was supp.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM ATX200R PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 Listing. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 195 PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific) LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific) LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 528L Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 223 Nylon 6, Nucleated A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon.. |
|||
Izod Impact, Notched | 0.530 - 5.30 J/cm | 0.993 - 9.93 ft-lb/in | Average value: 2.12 J/cm Grade Count:5 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Izod Impact, Notched | 0.530 J/cm - NB | 0.993 ft-lb/in - NB | Average value: 1.32 J/cm Grade Count:13 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R190H2 Acetal General purpose economy grade copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for maximum weatherability. Available in Natural and Black. Natural: Designated R190.. |
|||
Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
LG Chemical HI835H PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |