Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.450 J/cm | >= 0.843 ft-lb/in | ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 4341S Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Notched | 0.450 - 3.00 J/cm @Temperature -17.8 - 0.000 °C |
0.843 - 5.62 ft-lb/in @Temperature 0.000 - 32.0 °F |
Average value: 1.28 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.450 - 1.50 J/cm @Temperature -40.0 - 0.000 °C |
0.843 - 2.81 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.579 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.450 - 0.470 J/cm @Temperature -40.0 - -20.0 °C |
0.843 - 0.881 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.460 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
BASF Capron® B135QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
BASF Capron® B73QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | 1/8 in; ASTM Test |
BASF Capron® B85ZP Nylon 6 (DAM) (America)
(discontinued **) Not Impact modified.Information provided by BASF.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Loxim 330 12HSL Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.450 - 0.500 J/cm | 0.843 - 0.937 ft-lb/in | ASTM D256 |
Loxim 330 12V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | >= 0.450 J/cm | >= 0.843 ft-lb/in | Method A; ASTM D 256 |
Karina E 854-10/150-A-ERYB White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 0.000 °C |
0.843 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SPS Guang Zhou POBUXâ„¢ 3001G10 Flame-retarded/GF10%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Unitika M1030DH PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PA500 Nylon 6.6, Flame Retardant Flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA116 Nylon 6.6, Injection Molding polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer Polypropylene copolymer, high fluidityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -40.0 °C |
0.843 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |