Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.443 J/cm | 0.830 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Izod Impact, Notched | 0.443 J/cm | 0.830 ft-lb/in | ASTM D256 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |