Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP552N Fiber (Staple) Grade Polypropylene Moplen HP552N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552N is a homopolymer selected by customers for use in high speed.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed p.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP620M CPP Film Grade Polypropylene Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Izod Impact, Notched | 0.392 - 4.00 J/cm | 0.735 - 7.49 ft-lb/in | Average value: 1.77 J/cm Grade Count:104 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Izod Impact, Notched | 0.392 - 100 J/cm | 0.735 - 187 ft-lb/in | Average value: 7.09 J/cm Grade Count:113 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Engine Cover SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Shinil Chemical SHINSTAT PMMA Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.35 mm |
0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210P Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Zylog Hipolyene® 8001 SGM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm |
0.735 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30G25 POM, 25% Glass Fiber |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Zylog Hipolyene® 8021 MF HF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.392 J/cm - NB | 0.735 ft-lb/in - NB | Average value: 6.42 J/cm Grade Count:272 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 23.0 °C |
0.735 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |