Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.17 mm |
0.693 ft-lb/in @Thickness 0.125 in |
|
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific) CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 A 13 Black 13 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS (Asia Pacific) LNP* STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific) LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS (Asia Pacific) LNP* Thermocomp* CF008 is a compound based on Polystyrene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -40.0 °C |
0.693 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -40.0 °C |
0.693 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 264E0096908 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 22%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 71M Nylon 6, 40% Mineral Filled A 40% mineral reinforced Nylon 6 resin modified for reduced shrinkage.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R6020 Nylon 6 A medium viscosity extrusion grade resin with excellent melt stability and good melt strength, suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughn.. |
|||
Izod Impact, Notched | 0.370 - 1.33 J/cm | 0.693 - 2.50 ft-lb/in | Average value: 0.793 J/cm Grade Count:56 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |