Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.343 - 9.61 J/cm | 0.643 - 18.0 ft-lb/in | Average value: 6.22 J/cm Grade Count:215 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCON CP6062EX PC/ABS+CNT Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, .. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.343 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 0.643 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Izod Impact, Notched | >= 0.343 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 0.643 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | >= 0.343 J/cm @Temperature 23.0 °C |
>= 0.643 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H6007JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh rigidityHigh impact resistanceGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drink, bottles, pallet, garbage bins, con.. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
Cheng Yu Plastic PP225 Flame Retardant Polypropylene, Medium Impact |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F100 low-mid viscosity PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F101F Fast cycle time PBT Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good.. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30725 POM, 25% Mineral Reinforced |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | |
Zylog Hipolyene® 8021 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.343 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.643 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
LG Chemical HI835M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |