Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.304 - 0.900 J/cm | 0.570 - 1.69 ft-lb/in | Average value: 0.583 J/cm Grade Count:7 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.304 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.569 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.304 J/cm @Temperature 23.0 °C |
0.569 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% BARIUM SULPHATE REINFORCED HIGH GLOSS APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES |
|||
Izod Impact, Notched | 0.304 J/cm | 0.569 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N2020L Nanoclay 2% High flow Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Izod Impact, Notched | >= 0.304 J/cm | >= 0.569 ft-lb/in | ASTM D256 |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |