Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 J/cm @Temperature 23.0 °C |
0.401 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers SAN 300 Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 0.214 - 1.07 J/cm | 0.400 - 2.00 ft-lb/in | Average value: 0.492 J/cm Grade Count:21 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature 22.8 °C |
0.400 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
I. Stern PS2110 General Purpose Crystal Polystyrene Features:Moderately High Heat ResistanceUL Classification 94 HBExcellent Water ClarityApplicationsDisplaysHouse waresInformation provided by I. Stern & Co. Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
I. Stern WC-102 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 2600/2601 GPPS Foam extrusionLow residual styrene monomer contentModerate heat resistanceGood balance of strength and ease of processingUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolut.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 4181T Injection Molding Polypropylene Homopolymer with Antistat, ESCR AdditivesApplications: For general purpose injection molding applications such as closures.Formolene 4181T is a low viscosity, highly isotactic polypropylene homopoly.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.401 ft-lb/in | ASTM D256A |
Total PPH 3825WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3825WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Antistat - FINA 3.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
ExxonMobil PP1222F Mineral-filled Homopolymer Medium melt flow rate homopolymer, 20% filled. Particularly suitable for consumer products and appliance applications requiring long term heat aging resistance. UL continuous service rating of 95°.. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.401 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 300 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics EA3400 High Heat Crystal Polystyrene Product CharacteristicsLess than 300 parts per million residual volatiles with minimal taste and odor transferExcellent clarity and colorGood toughnessFood Contact CompliantTypical ApplicationsCap l.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics MC3650 High Heat Crystal Polystyrene Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P-40TC-2767 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.400 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ ES-5500C TC-EM Polyethersulfone
(discontinued **) Description/Features:Thermally ConductiveCeramic FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.214 - 0.740 J/cm | 0.401 - 1.39 ft-lb/in | Average value: 0.462 J/cm Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |