Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.155 - 0.481 J/cm | 0.290 - 0.900 ft-lb/in | Average value: 0.286 J/cm Grade Count:4 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched | 0.155 J/cm | 0.290 ft-lb/in | ASTM D256 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Izod Impact, Notched | 0.155 J/cm | 0.290 ft-lb/in | ASTM D256 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Izod Impact, Notched | 0.155 J/cm | 0.290 ft-lb/in | |
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation con.. |
|||
Izod Impact, Notched | 0.155 J/cm | 0.290 ft-lb/in | |
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system.. |
|||
Izod Impact, Notched | 0.155 J/cm | 0.290 ft-lb/in | ASTM D256 |
Plenco 4311 Phenolic, Granular, Injection Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |