Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.110 - 0.160 J/cm | 0.206 - 0.300 ft-lb/in | ASTM D256 |
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign.. |
|||
Izod Impact, Notched | <= 0.110 J/cm | <= 0.206 ft-lb/in | ASTM D256 |
Proto3000 CastForm™ PS Selective Laser Sintering (SLS®) Prototyping Polymer Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short bur.. |
|||
Izod Impact, Notched | 0.110 J/cm | 0.206 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Izod Impact, Notched | 0.110 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.206 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene HI650 Polystyrene APPLICATIONS: INJECTION MOULDING, ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARES. etc. |
|||
Izod Impact, Notched | 0.110 - 0.160 J/cm | 0.206 - 0.300 ft-lb/in | ASTM D256 |
3D Systems Accura® 45HC Plastic for SLA® Systems A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho.. |
|||
Izod Impact, Notched | 0.110 J/cm | 0.206 ft-lb/in | ASTM D256 |
ALM PS 200 Prototyping Polymer Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor.. |
|||
Izod Impact, Notched | 0.110 J/cm @Thickness 3.20 mm |
0.206 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | <= 0.110 J/cm | <= 0.206 ft-lb/in | ASTM D256 |
3D Systems CastForm™ PS Plastic for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo.. |
|||
Izod Impact, Notched | 0.110 J/cm @Temperature 23.0 °C |
0.206 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.110 J/cm @Temperature 23.0 °C |
0.206 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 152 Fiber Extrusion Polypropylene Applications: Nonwoven by blow process for disposable diapers, personal care and disposable medical care. Information provided by Braskem |
|||
Izod Impact, Notched | 0.110 - 5340 J/cm | 0.206 - 10000 ft-lb/in | Average value: 0.756 J/cm Grade Count:109 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |