Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.0850 J/cm | 0.159 ft-lb/in | ISO 180 Method A |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Izod Impact, Notched | 0.0850 J/cm @Temperature 23.0 °C |
0.159 ft-lb/in @Temperature 73.4 °F |
ISO 180/A |
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.0850 J/cm - NB | 0.159 ft-lb/in - NB | Average value: 4.49 J/cm Grade Count:155 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |