Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.0400 - 1.01441 J/cm @Temperature -40.0 - 0.000 °C |
0.0749 - 1.90041 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.494 J/cm Grade Count:62 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0400 J/cm @Temperature -40.0 °C |
0.0749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |