| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific) Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating.. |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
| SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | 50%RH; ISO 179/1eA |
| DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
| Charpy Impact, Notched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179 |
| Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
Dry; ISO 179/Af |
| Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
| Charpy Impact, Notched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||