| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -40.0 °C |
1.81 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
| Nilit FRIANYL A63 N-SG5 Nylon 6.6 for injection molding, 5% mineral filled Nylon 6.6 for injection molding, low viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | |
| Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66 Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
ISO data |
| BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8200 HS BK-102 is a medium viscosity, heat stabilized, pigmented black, nylon 6 injection molding homopolymer exhibiting resistance to sink-mark formation in thick section, and improved tough.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -20.0 °C |
1.81 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
| Global PP-2300-NCA Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperature, UV stabilizerApplications-automotive, electrical appliancesInformation provided by Global Polymers Corporation.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ASTM D256 |
| Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179 |
| Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179 |
| Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179-1 |
| Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | Bayer Test |
| Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179/1eA |
| DuPont Performance Polymers Crastin® S650FR BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced black flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Perfor.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179/1eA |
| DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
|
| Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
|
| Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
|
| Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | 1eA; ISO 179 |
| Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
| Charpy Impact, Notched | >= 0.380 J/cm² @Temperature 23.0 °C |
>= 1.81 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| AKG Polymers Vision PP PPH BL3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
| Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179 |
| BASF Ultramid® N-276 NF3001 40% Glass/Mineral Filled PA66 (Dry) Ultramid N-276 NF3001 is a 40% mineral/glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
| Charpy Impact, Notched | >= 0.380 J/cm² @Temperature 23.0 °C |
>= 1.81 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| AKG Polymers Vision PP PPH TC3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | ISO 179/1eA |
| BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |
|||
| Charpy Impact, Notched | 0.380 - 2.30 J/cm² | 1.81 - 10.9 ft-lb/in² | Average value: 0.890 J/cm² Grade Count:46 |
| Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
| Charpy Impact, Notched | 0.380 - 3.20 J/cm² | 1.81 - 15.2 ft-lb/in² | Average value: 1.43 J/cm² Grade Count:9 |
| Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |
|||
| Charpy Impact, Notched | 0.380 J/cm² | 1.81 ft-lb/in² | |
| LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||