Charpy Impact, Notched 60.0 - 100 J/cm²
286 - 476 ft-lb/in²
Plansee DENAL® 910 179 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Charpy Impact, Notched 60.0 - 100 J/cm²
286 - 476 ft-lb/in²
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.