Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.650 - 10.0 J/cm² | 3.09 - 47.6 ft-lb/in² | Average value: 2.30 J/cm² Grade Count:43 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.650 - 10.0 J/cm² | 3.09 - 47.6 ft-lb/in² | Average value: 4.80 J/cm² Grade Count:50 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 2.40 - 10.0 J/cm² | 11.4 - 47.6 ft-lb/in² | Average value: 4.60 J/cm² Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Charpy Impact, Notched | 0.200 - 10.0 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 47.6 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.17 J/cm² Grade Count:23 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 5.00 - 10.0 J/cm² | 23.8 - 47.6 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Charpy Impact, Notched | 8.00 - 10.0 J/cm² | 38.1 - 47.6 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Charpy Impact, Notched | 0.300 - 10.0 J/cm² | 1.43 - 47.6 ft-lb/in² | Average value: 1.24 J/cm² Grade Count:20 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |