Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.50 - 4.00 J/cm² @Temperature 23.0 °C |
11.9 - 19.0 ft-lb/in² @Temperature 73.4 °F |
depending on color; ISO 179/1eA |
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.360 - 4.00 J/cm² | 1.71 - 19.0 ft-lb/in² | Average value: 1.37 J/cm² Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.600 - 4.00 J/cm² | 2.86 - 19.0 ft-lb/in² | Average value: 2.02 J/cm² Grade Count:113 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Charpy Impact, Notched | 0.550 - 4.00 J/cm² | 2.62 - 19.0 ft-lb/in² | Average value: 1.64 J/cm² Grade Count:8 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact, Notched | 0.600 - 4.00 J/cm² | 2.86 - 19.0 ft-lb/in² | Average value: 2.15 J/cm² Grade Count:21 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact, Notched | 3.00 - 4.00 J/cm² | 14.3 - 19.0 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p.. |
|||
Charpy Impact, Notched | 0.300 - 4.00 J/cm² @Temperature -30.0 - -20.0 °C |
1.43 - 19.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.34 J/cm² Grade Count:7 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact, Notched | 0.400 - 4.00 J/cm² @Temperature -30.0 - -20.0 °C |
1.90 - 19.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 2.71 J/cm² Grade Count:14 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |