Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.700 - 3.20 J/cm² | 3.33 - 15.2 ft-lb/in² | Average value: 1.23 J/cm² Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact, Notched | 0.600 - 3.20 J/cm² | 2.86 - 15.2 ft-lb/in² | Average value: 1.58 J/cm² Grade Count:39 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Charpy Impact, Notched | 0.300 - 3.20 J/cm² | 1.43 - 15.2 ft-lb/in² | Average value: 0.979 J/cm² Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact, Notched | 1.60 - 3.20 J/cm² | 7.61 - 15.2 ft-lb/in² | Average value: 2.22 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 1.60 - 3.20 J/cm² @Temperature -30.0 - -30.0 °C |
7.61 - 15.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.22 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.380 - 3.20 J/cm² | 1.81 - 15.2 ft-lb/in² | Average value: 1.43 J/cm² Grade Count:9 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |