Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 3.00 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 14.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.25 J/cm² Grade Count:29 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 0.500 - 3.00 J/cm² | 2.38 - 14.3 ft-lb/in² | Average value: 1.62 J/cm² Grade Count:19 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Charpy Impact, Notched | 1.50 - 3.00 J/cm² @Temperature -30.0 - 30.0 °C |
7.14 - 14.3 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.29 J/cm² Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Charpy Impact, Notched | 0.400 - 3.00 J/cm² | 1.90 - 14.3 ft-lb/in² | Average value: 1.21 J/cm² Grade Count:30 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact, Notched | 3.00 - 3.00 J/cm² @Temperature -20.0 - -20.0 °C |
14.3 - 14.3 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.00 J/cm² Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact, Notched | 0.300 - 3.00 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 14.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.10 J/cm² Grade Count:24 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.300 - 3.00 J/cm² | 1.43 - 14.3 ft-lb/in² | Average value: 1.25 J/cm² Grade Count:71 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 0.600 - 3.00 J/cm² | 2.86 - 14.3 ft-lb/in² | Average value: 1.44 J/cm² Grade Count:13 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Charpy Impact, Notched | 2.50 - 3.00 J/cm² | 11.9 - 14.3 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Charpy Impact, Notched | 1.80 - 3.00 J/cm² | 8.57 - 14.3 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Charpy Impact, Notched | 1.80 - 3.00 J/cm² | 8.57 - 14.3 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote.. |
|||
Charpy Impact, Notched | 0.400 - 3.00 J/cm² | 1.90 - 14.3 ft-lb/in² | Average value: 1.42 J/cm² Grade Count:69 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.600 - 3.00 J/cm² @Temperature -30.0 - -30.0 °C |
2.86 - 14.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.30 J/cm² Grade Count:10 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |