Polymer Property : Charpy Impact, Notched = 13.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.100 - 2.90 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 13.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.28 J/cm² Grade Count:69
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..