Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Akulon® PA 66 - Akulon 66 - at 50% RH Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD4271 PC Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
Ineos ABS Lustran® H606 LS Improved heat and UV resistance.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
Ineos ABS Lustran® LGM Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO Data |
Styron Pulse® 959 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO Data |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 30.0 °C |
8.57 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50 Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 300TE BK602 Acetal (POM)
(Unverified Data**) Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE BK602 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin 30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® CLG357 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl C2 ZV40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Charpy Impact, Notched | >= 1.80 J/cm² | >= 8.57 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |